One question that comes up quite often in regard to this semi dry mix is the cement content.
Semi dry concrete mix.
By the time you get the repair material mixed it will be ready.
This helps to keep the mix free from stones or dirt on the floor and also avoids leaving a concrete stain.
For the pointing i was going to leave the slabs to set for 24 hrs and then do another mix of damp mortar with ratio of 3 1 sand cement is this ok.
Another thing im not sure on is the spacing to leave in between the slabs 5mm or 10mm.
The semi dry mix tends not to be picked up and carried by tools and boots so there less risk of accidentally staining the flags during the laying process.
This is referred to as a moist mix and probably the most useful and most commonly specified consistence.
It is not necessary for this scratch coat to dry.
This applies to pre mix as well.
Dry lean semi dry mix cement bound material consisting of cement 4 20mm stone graded sand and minimal water.
It is always best to mix concrete or mortar on a piece of board spot board.
Mixing concrete and mortar.
Dry lean semi dry mix cement bound material consisting of cement 4 20mm stone graded sand and minimal water.
The chemical approach involved mixing up a liquid bonding agent that helps bond new concrete products to old.
Start by mixing the separate components thoroughly whilst dry.
This dry mix seems a lot easier than using the damp mix and would take a lot less time.
Then mix up additional repair material to the proper consistency and apply over this thin scratch coat.
This is sometimes referred to as semi dry.
Maxileanmix is a semi dry ready mixed concrete that s ideal for projects where strength is not a key factor.